The Basics Of Fiberglass Fabrication - How To
|
Stir the MEKP into the resin using a stir stick for at least 30 seconds for proper mixing. The mixture should change color. You should have 20 to 30 minutes of working time at 70 degrees. If it starts to gel before then, mix up a new batch, adjusting the amount of hardener by 15 to 25 percent (do not use resin that has begun to gel) View Related Article
|
|